bob

Posted

Feb 23 at 07:33 PM

Finaly made the core suport and layed my intercooler pipes and was able to do it just thinking I may try and make the pipes with less boots

Posted

Feb 19 at 10:52 PM

I finaly decided to try some intercooler pipe. I got some cuts layed out and geting ready to tack it up.the last try looked like burnt or sunken in a few dabs was at 90 amp 3/32 and the 100hz and 45 % I am new at this so my macine starts at 25% and I believe to 80 were should the sweet spot be this China box instructions are impossible like my message

2

Posted

Feb 03 at 05:37 PM

Playing with aluminum is the black soot loss of coverage or diping tungsten

4

Posted

Jan 26 at 06:57 PM

1 / 3
2 / 3
3 / 3

New to tig welding .got a new tig ac dc inverter box from over seas it's got lots of features almost overwhelming I also have a 64 ford f100 swb that I 4linked and built a twin turbo 472 and now working on plumbing and have to learn aluminum and stanless

3